What is Lack of Fusion in welding defects?

This question was previously asked in
RRB JE CBT 2 (Mechanical Engineering) ReExam Official Paper (Held On: 04 Jun, 2025)
View all RRB JE Papers >
  1. It is the failure of the filler metal to penetrate into the welding joint.
  2. It is the entrapment of slag or other impurities in the weld. 
  3. It is the failure of the filler metal to fuse with the parent metal.
  4. It is a group of small holes throughout the weld metal.

Answer (Detailed Solution Below)

Option 3 : It is the failure of the filler metal to fuse with the parent metal.
Free
General Science for All Railway Exams Mock Test
2.2 Lakh Users
20 Questions 20 Marks 15 Mins

Detailed Solution

Download Solution PDF

Explanation:

Lack of Fusion in Welding Defects

  • Lack of fusion is a critical welding defect that occurs when the filler metal fails to properly fuse with the parent (base) metal or between layers of weld metal in a multi-pass weld. This defect compromises the structural integrity of the weld and can lead to failures under stress or load. Proper fusion is essential to ensure that the weld achieves the desired strength, durability, and performance characteristics.
  • In welding, the process involves melting the base metal and filler material to create a strong bond. Lack of fusion typically arises when there is inadequate heat input, improper welding technique, contamination, or poor joint preparation. The defect is characterized by visible or subsurface separation at the weld interface, indicating that the materials did not bond effectively.

Causes of Lack of Fusion:

  • Low Heat Input: Insufficient heat during the welding process prevents the base metal and filler material from reaching the appropriate temperature required for fusion.
  • Improper Welding Technique: Incorrect manipulation of the welding torch, electrode, or filler material can result in poor bonding between the materials.
  • Contamination: The presence of dirt, grease, rust, or other impurities on the welding surfaces can inhibit proper bonding.
  • Incorrect Welding Parameters: Using incorrect current, voltage, or travel speed can lead to insufficient penetration and fusion.
  • Improper Joint Preparation: Inadequate cleaning, poor fit-up, or incorrect joint design can contribute to lack of fusion.

Impact of Lack of Fusion:

  • Reduction in the overall strength of the weld joint.
  • Increased susceptibility to crack propagation and failure under load or stress.
  • Compromised fatigue resistance, especially in dynamic or cyclic loading conditions.
  • Potential safety hazards in critical applications, such as bridges, pipelines, and pressure vessels.

Detection of Lack of Fusion:

  • Visual Inspection: Surface lack of fusion may be visible as a distinct line or separation at the weld interface.
  • Non-Destructive Testing (NDT): Techniques such as ultrasonic testing, radiographic testing, or dye penetrant testing can identify subsurface or internal lack of fusion.

Prevention of Lack of Fusion:

  • Use appropriate welding parameters, including correct current, voltage, and travel speed.
  • Ensure proper cleaning and preparation of the base metal and filler material before welding.
  • Adopt correct welding techniques and ensure proper torch or electrode manipulation.
  • Increase heat input where necessary to achieve better penetration and fusion.
  • Conduct regular training and skill development for welders to minimize defects due to human error.
Latest RRB JE Updates

Last updated on Jul 21, 2025

-> The RRB JE CBT 2 Result 2025 has been released on July 21, 2025 for all RRBs Zones (Ahmedabad, Bengaluru, Jammu-Srinagar, Kolkata, Malda, Mumbai, Ranchi, Secunderabad, and Thiruvananthapuram).

-> RRB JE CBT 2 Scorecard 2025 has been released along with cut off Marks.

-> RRB JE CBT 2 answer key 2025 for June 4 exam has been released at the official website.

-> Check Your Marks via RRB JE CBT 2 Rank Calculator 2025

-> RRB JE CBT 2 admit card 2025 has been released. 

-> RRB JE CBT 2 city intimation slip 2025 for June 4 exam has been released at the official website.

-> RRB JE CBT 2 Cancelled Shift Exam 2025 will be conducted on June 4, 2025 in offline mode. 

-> RRB JE CBT 2 Exam Analysis 2025 is Out, Candidates analysis their exam according to Shift 1 and 2 Questions and Answers.

-> The RRB JE Notification 2024 was released for 7951 vacancies for various posts of Junior Engineer, Depot Material Superintendent, Chemical & Metallurgical Assistant, Chemical Supervisor (Research) and Metallurgical Supervisor (Research). 

-> The selection process includes CBT 1, CBT 2, and Document Verification & Medical Test.

-> The candidates who will be selected will get an approximate salary range between Rs. 13,500 to Rs. 38,425.

-> Attempt RRB JE Free Current Affairs Mock Test here

-> Enhance your preparation with the RRB JE Previous Year Papers

Get Free Access Now
Hot Links: teen patti master 2025 teen patti bonus teen patti vip